①原料描述部分 |
|||
规格级别 |
注塑 |
外观颜色 |
|
该料用途 |
|
||
备注说明 |
类型:尼龙-6未强化,标准等级 |
②加工条件 |
加工条件 |
|
③原料技术数据
性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
||||
基本性能 |
吸水率 |
23℃,24小时 |
ASTM D-570 |
|
% |
|||
物理性能 |
泰伯磨耗量 |
1000g,CS-17 |
ASTM D-1044 |
|
mg/1000次 |
|||
比重 |
ASTM D-792 |
|
||||||
机械性能 |
IZOD冲击强度 |
无缺口1/2",23℃ |
|
kg.cm/cm |
||||
IZOD冲击强度 |
-40℃,无缺口1/2 |
|
kg.cm/cm |
|||||
断裂伸长率 |
23℃ |
ASTM D-638 |
|
% |
||||
搞剪强度 |
23℃ |
ASTM D-732 |
|
Kg/cm2 |
||||
挠曲强度 |
80℃ |
ASTM D-790 |
|
Kg/cm2 |
||||
挠曲强度 |
-40℃ |
ASTM D-790 |
|
Kg/cm2 |
||||
洛氏硬度 |
23℃ |
ASTM D-785 |
|
|||||
抗拉屈服强度 |
23℃ |
ASTM D-638 |
|
Kg/cm2 |
||||
抗拉屈服强度 |
80℃ |
ASTM D-638 |
|
Kg/cm2 |
||||
抗拉屈服强度 |
-40 |
ASTM D-638 |
|
Kg/cm2 |
||||
挠曲模量 |
-40℃ |
ASTM D-790 |
|
Kg/cm2 |
||||
抗拉断裂强度 |
23℃ |
ASTM D-638 |
|
Kg/cm2 |
||||
挠曲模量 |
23℃ |
ASTM D-790 |
|
Kg/cm2 |
||||
压缩强度 |
23℃ |
ASTM D-695 |
|
Kg/cm2 |
||||
洛氏硬度 |
23℃ |
ASTM D-785 |
|
|||||
挠曲强度 |
23℃ |
ASTM D-790 |
|
Kg/cm2 |
||||
挠曲模量 |
80℃ |
ASTM D-790 |
|
Kg/cm2 |
||||
IZOD冲击强度 |
23℃,无缺口1/8 |
|
kg.cm/cm |
|||||
电气性能 |
体积电阻率 |
ASTM D-257 |
|
Ω.cm |
||||
损耗因素 |
106Hz |
ASTM D-150 |
|
|||||
介电强度 |
1/8" |
ASTM D-149 |
|
KV/mm |
||||
损耗因素 |
50Hz |
ASTM D-150 |
|
|||||
IEC导电径踪指数 |
UL 746 |
|
V |
|||||
介电常数 |
106Hz |
ASTM D-150 |
|
|||||
损耗因素 |
103Hz |
ASTM D-150 |
|
|||||
抗电弧性 |
1/8" |
ASTM D-150 |
|
|||||
介电常数 |
50HZ |
ASTM D-150 |
|
|||||
介电常数 |
106Hz |
ASTM D-150 |
|
|||||
热性能 |
导热系数 |
|
Kcal/m.hr.°C |
|||||
线性热膨胀系数 |
ASTM D-696 |
|
10-5cm/cm.℃ |
|||||
比热 |
|
Cal/g.°C |
||||||
热挠曲温度 |
ASTM D-648 |
|
℃ |
|||||
熔点 |
差示扫描测热计DSC法 |
|
℃ |
|||||
UL-94抗燃级 |
UL 94 |
|
||||||
热挠曲温度 |
18.6kg/cm2 |
ASTM D-648 |
|