1.停车场划线施工前要结合实际地形结构,统计车辆预留车库数量做好准备工作,线形流畅,开线要准,路面要干燥,除净灰尘、杂物等。http://www.hxjzazgc.com 济南车库划线 1 parking crossed before construction should be combined with the actual terrain structure, statistical vehicle reservation garage quantity prepare, streamline, line to be accurate, the pavement to dry, in addition to dust and sundries. 2.停车场划线涂料在釜内加热时,温度应控制在180℃~220℃,同时充分搅拌,涂料完全熔化后,保温搅拌5分钟,即可进行施工。 2 parking marking coating is heated in a kettle, temperature should be controlled at 180 DEG ~220 DEG, and fully mixing, coating compleby after melting, heat preservation stirring for 5 minutes, can carry out construction. 3.非同类涂料不得混合,需将釜内清理干净后才能换用另一种涂料待下涂剂完全干燥后划线,水泥路面和老化、板结的沥青路面喷涂一遍后需喷涂第二遍。http://www.hxjzazgc.com 3 non similar coating shall not be required to be mixed, kettle after cleaning, can be replaced with another kind of paint to dry compleby pigmentum after marking, asphalt pavement cement concrete pavement and aging, hardening spraying again after spraying second times 4.气温过低和路面潮湿时不宜施工,随时检查施工作业,如标线厚度、外观等是否符合要求,坚持做施工记。