瑞典伊萨OK TIGROD 55、ER100S-G低合金钢焊条
分类
SFA/AWS A5.28 |
ER100S-G |
EN 16834-A |
Mn3NiCrMo |
测试温度(焊态) | 0 °C |
结果(焊态) | 150 J |
测试温度(焊态) | -20 °C |
结果(焊态) | 85 J |
伸长率(焊态) | 27 % |
屈服强度(焊态) | 585 MPa |
抗拉强度(焊态) | 750 MPa |
电流类型 CA/CD/CC (+)(-) | DC(-) |
元素 | C |
额定百分比 | 0.085 % |
元素 | Si |
额定百分比 | 0.7 % |
A copper coated, low alloyed, chromium-nickel-molybdenum (0,5% Cr, 0,5% Ni, 0,2% Mo) rod for GTAW of high strength steels with a minimum tensile strength of 690 MPa. The rod is also suitable for welding of steels where a good impact strength at low temperatures is required.