比重 | 1.24 | g/cm | ASTM D792 |
硬度 | 70 | ASTM D2240 |
断裂延伸率 | 4.957 | MPa | ASTM D573 |
6.27 | MPa | ASTM D412 | |
拉伸应力 - 横向流量 | 2.69 | MPa | ASTM D412 |
伸长率 | 412.5 | % | ASTM D573 |
550 | % | ASTM D412 |
介电强度 | 2.50 | ASTM D150 | |
介电常数 | 31.9 | kV/mm | ASTM D149 |
极限氧指数 | 26.0 | % | ASTM D2863 |
加工温度 | 175-230 | ℃ | |
模具温度 | 10.0-51.7 | ℃ | |
干燥温度 | 82.2 | ℃ | |
干燥时间 | 3 | hr | |
建议的大水分含量 | 0.0800 | % | |
支撑强度 | 0.345-0.689 | MPa | |
背压 | 41.4-68.9 | MPa | |
排气孔深度 | 0.00254 | cm | |
垫层 | 0.317-0.635 | cm | |
螺杆转速 | 100-200 | rpm |